Components requiring excellent resistance to boiling, concentrated nitric acid, equipment and components exposed to highly concentrated chlorine solutions at elevated temperatures, components for urea plants.
Austenitic chromium-nickel-molybdenum steel with nitrogen addition and extra low carbon content. Resistant to intergranular corrosion in the temperature range up to 400°C. Does not require post-weld heat treatment. Surface finish required for optimum corrosion resistance: pickled. Cold forming properties are very good. The steel is capable of taking a mirror polish.
DIN | UNS | EN | Others |
---|---|---|---|
1.4466 | S31050 | X1CrNiMoN25-22-2 | AISI: 310 MoLN |
Si | Mn | Cr | Mo | Ni | N | |
---|---|---|---|---|---|---|
0.30 | 1.80 | 25.00 | 2.20 | 22.00 | 0.12 |